T1 - Influencia de la adición de viruta de acero en la resistencia a compresión en ladrillos artesanales en prismas de albañileria
AU - Yahira, Hernandez Rodriguez Jasmin
AU - Jorginho, Vaca Rodriguez John
AU - Germán, Sagástegui Vásquez
N1 - Publisher Copyright:
© 2023 Latin American and Caribbean Consortium of Engineering Institutions. All rights reserved.
PY - 2023
Y1 - 2023
N2 - This research aims to determine the influence of the addition of steel shavings (VA) on the compressive strength of artisan bricks in masonry prisms, for which 30 prisms were made, each prism made up of three bricks and a 1.5 joint. cm, 6 of these for each percentage that was 0%, 5%, 10%, 15% and 20% addition of steel chips. The research is experimental and according to its nature it is quantitative. The results indicate that for an addition of 15% (V.A.), the compressive strength in brick units increases and is optimal, resulting in 74.31 kg/cm2 unlike the standard brick, which is 54.33 kg/cm2; In prisms the same thing happens for an addition of 15% (V.A.) the compressive strength reaches 49.30 kg/cm2 unlike the standard prism which is 23.88 kg/cm2 however, if the resistances are added to more than this percentage they start to go down. It was concluded that the influence of the addition of (V.A.) in handmade bricks and masonry prisms has a positive influence, improving this property by 206.44% with respect to the standard prisms, but up to 15% of addition of (V.A.).
AB - This research aims to determine the influence of the addition of steel shavings (VA) on the compressive strength of artisan bricks in masonry prisms, for which 30 prisms were made, each prism made up of three bricks and a 1.5 joint. cm, 6 of these for each percentage that was 0%, 5%, 10%, 15% and 20% addition of steel chips. The research is experimental and according to its nature it is quantitative. The results indicate that for an addition of 15% (V.A.), the compressive strength in brick units increases and is optimal, resulting in 74.31 kg/cm2 unlike the standard brick, which is 54.33 kg/cm2; In prisms the same thing happens for an addition of 15% (V.A.) the compressive strength reaches 49.30 kg/cm2 unlike the standard prism which is 23.88 kg/cm2 however, if the resistances are added to more than this percentage they start to go down. It was concluded that the influence of the addition of (V.A.) in handmade bricks and masonry prisms has a positive influence, improving this property by 206.44% with respect to the standard prisms, but up to 15% of addition of (V.A.).
KW - Compressive Strength
KW - Prisms
KW - Steel Chips (V.A..)
KW - influence
UR - http://www.scopus.com/inward/record.url?scp=85172392129&partnerID=8YFLogxK
M3 - Contribución a la conferencia
AN - SCOPUS:85172392129
T3 - Proceedings of the LACCEI international Multi-conference for Engineering, Education and Technology
BT - Proceedings of the 21st LACCEI International Multi-Conference for Engineering, Education and Technology
A2 - Larrondo Petrie, Maria M.
A2 - Texier, Jose
A2 - Matta, Rodolfo Andres Rivas
T2 - 21st LACCEI International Multi-Conference for Engineering, Education and Technology, LACCEI 2023
Y2 - 19 July 2023 through 21 July 2023
ER -